Skip to content

Marbling

Featured Replies

Looking for some insite on marbling. What epoxies seem to be best "i would assume high build" or what pigments to use. Also if you have any techniques you want to share it would be much appreciated

  • Super User

I use high build and timing is everything for different effects from the marbling.  I have CRB pigments and testors model paint.  

  • Super User

Ok. What does timing have to do with it? I guess ill have to practis

 

From the time you get it mixed, the consistency of the finish gets thicker by the minute until it sets. The longer you wait to add the finish mixed with the pigment, the sharper and more defined the marbling will be.  The earlier you do it, the more fluid the mix is, and it moves and blends more.  The great thing about marbling is you never quite know for sure how it's going to look until the next day when it's dry.

  • Super User

From the time you get it mixed, the consistency of the finish gets thicker by the minute until it sets. The longer you wait to add the finish mixed with the pigment, the sharper and more defined the marbling will be.  The earlier you do it, the more fluid the mix is, and it moves and blends more.  The great thing about marbling is you never quite know for sure how it's going to look until the next day when it's dry.

 

That, for me, is the problem. I have an idea, or a look I'm going for, then get something I like, and the next day it's different. Been working on scrap pieces of blank, not on any real rods so far.

 

It seems simple; wait until the epoxy has thickened a bit and proceed. Do it too soon, and it all runs together. So, wait longer, right? Wait long enough to get some decent separation, and you get threads stringing out from the tool that go anywhere except where you want them to go.

 

I'll keep experimenting. I've seen some that look really good. It may be a while before I get to that point.

Much like guide wrap finishing, you just have to experiment and find what works for you. There are so many variables it's hard to say for someone else. So far, Flex Coat High Build has a pot life and consistency that works well at around 70*F room temp. 

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.
Note: Your post will require moderator approval before it will be visible.

Guest
Unfortunately, your content contains terms that we do not allow. Please edit your content to remove the highlighted words below.
Reply to this topic...

Recently Browsing 0

  • No registered users viewing this page.

Important Information

We have placed cookies on your device to help make this website better. You can adjust your cookie settings, otherwise we'll assume you're okay to continue.

Account

Navigation

Search

Search

Configure browser push notifications

Chrome (Android)
  1. Tap the lock icon next to the address bar.
  2. Tap Permissions → Notifications.
  3. Adjust your preference.
Chrome (Desktop)
  1. Click the padlock icon in the address bar.
  2. Select Site settings.
  3. Find Notifications and adjust your preference.